2.4 Plasticizers

A plasticizer turns rigid PVC into the soft, flexible material used in PVC coated fabric and also makes the compound easier to process. Plasticizer content is measured in PHR, or parts per hundred parts of PVC resin. In tarpaulin and coated fabric, it usually ranges from about 20 to 80 PHR, and most calendering plants work at around 70 PHR.

Plasticizer Level Lower PHR (toward 20) Higher PHR (toward 80)
Hand Feel Firmer, stiffer Softer, more supple
Low-Temperature Performance Stiffens and cracks more easily in the cold Stays flexible at lower temperatures
Cost Lower Higher

Plasticizer that is poorly matched to the formula can migrate to the surface of the finished fabric, leaving it sticky or oily. Choosing the right plasticizer type and level, and balancing it with the rest of the formula, prevents this.

The plasticizer is also what most buyers are really asking about when they ask whether a vinyl fabric is non-toxic or eco-friendly. The answer depends on which plasticizer is used and which regulation the fabric is tested against.

2.4.1 Phthalate Plasticizers

Phthalate plasticizers are mature and low in cost, but because of environmental and safety concerns, their use is increasingly restricted in sensitive applications. In the United States, for example, CPSC rules prohibit children’s toys and child care articles from containing more than 0.1% of eight listed phthalates in any accessible plasticized part.

Plasticizer Characteristics Advantages Limitations
DOP (DEHP) General-purpose plasticizer with balanced performance; good compatibility with PVC and easy to process The most mature technology at low cost; the most widely used plasticizer in the tarpaulin industry A phthalate under scrutiny; restricted in sensitive uses such as children’s toys and food contact. Average durability and cold resistance
DINP Outperforms DOP with lower volatility and better aging resistance Better durability and migration resistance than DOP; one of the main upgrades from DOP Still a phthalate; less controversial than DOP but restricted under some strict environmental standards. Average cold resistance
DPHP High-performance phthalate with excellent durability and electrical insulation Very low volatility and excellent heat and aging resistance; well suited to premium tarpaulins with long service requirements Still a phthalate and costs more than DOP and DINP. Cold resistance is not its strength

2.4.2 Non-Phthalate Plasticizers

Driven by environmental regulations, non-phthalate plasticizers have become the mainstream trend, especially for exported fabrics and customers with environmental requirements.

Plasticizer Characteristics Advantages Limitations
DOTP Non-phthalate and one of the most widely used eco-friendly plasticizers, with strong all-round performance Meets RoHS, REACH and similar requirements; good electrical insulation, heat resistance and low volatility Costs more than DOP; slightly lower compatibility with PVC, so the formula needs adjusting. Average cold resistance
TOTM Non-phthalate, high-performance, high-heat plasticizer Excellent heat resistance, durability and low migration; a first choice for premium heat-resistant tarpaulins and automotive interiors Expensive and needs higher processing temperatures
DOA / DOS Non-phthalate plasticizers designed for cold resistance Significantly improve low-temperature performance, keeping the fabric soft in cold conditions Poor compatibility with PVC and migrate easily, so they are blended with a primary plasticizer such as DOTP rather than used alone

LonaTarp has a stable supply of DOTP and other eco-friendly plasticizers, and the related test reports are available for your review.

2.4.3 Plasticizer Blends

In production, a tarpaulin formula usually combines several plasticizers to balance performance and cost. Typical systems:

Goal Plasticizer System Notes
Cost-Effective General Use DINP or DOTP as the primary plasticizer, replacing DOP Balances price and performance for standard covers
Export Markets with Strict Regulations DOTP or TOTM as the primary plasticizer For phthalate-free vinyl fabric
Cold Resistance DOTP or DINP plus 5–15 PHR of DOA or DOS For winter transport, cold storage and cold climates
Maximum Durability DPHP if phthalates are acceptable; TOTM if the product must be phthalate-free For long outdoor service and heat exposure

For PVC coating on fabric for low temperatures, the plasticizer system matters most: a DOA or DOS addition keeps the coating flexible where a standard formula would stiffen and crack.

2.4.4 Specifying a Phthalate-Free or Compliant Order

“Eco-friendly material” is not a specification. “3P”, “6P” and “16P” are industry shorthand for groups of phthalates; 6P, for example, usually covers DEHP, BBP, DBP, DNOP, DIDP and DINP. Formal compliance is judged by your target market, the product’s use, the test report and the current version of the regulation. The EU REACH SVHC Candidate List, for instance, is updated regularly, and RoHS applies to electrical and electronic equipment rather than to every fabric. To formulate and test the right material, we need the following:

Item What to Tell Us
Target Market EU, United States, United Kingdom, Japan or a customer’s internal standard
Product Use General industrial, children’s products, mattresses, sports mats, food contact or medical-adjacent use
Test Items 3P, 6P, 16P, RoHS, REACH SVHC or another list
Third-Party Testing Whether a third-party report is required, and any specified laboratory or report validity

Production equipment and the workshop environment can carry traces of plasticizers from earlier runs. For a phthalate-free order at or near the minimum quantity, we take test samples from the end of the production run, where the risk of carry-over is lowest.

Send us your market and test list, and we will match the plasticizer system and confirm it on a trial sample before bulk production.