2.5 Fillers
Fillers are mineral powders added to the PVC coating compound. The most common is calcium carbonate, often called calcium powder in the industry. Used in the right amount, it improves processing flow, thermal stability, hardness and stiffness while lowering cost. Used in excess, it reduces flexibility and tear strength, makes white crease marks (stress whitening) more visible when the fabric is folded, and shortens the service life of the finished product.
| Filler | Main Benefits | When It Is Used |
|---|---|---|
| Calcium Carbonate | Improves processing flow, thermal stability, hardness and stiffness while lowering cost | The standard filler for PVC coated fabric |
| Barium Sulfate | An alternative to calcium carbonate, and commonly used as a filler in plastics | Applications where the fabric is in contact with acidic substances |
Particle size also affects the result. A study published in Materials Research found that combining micro- and nano-sized calcium carbonate in a PVC matrix gave better overall properties than using either size alone.
2.5.1 How Much Filler Is Used
Like other ingredients, filler is measured in PHR, or parts per hundred parts of PVC resin. The level varies widely across the market, and it is one of the main reasons two fabrics of the same weight can differ so much in price and performance.
| Calcium Carbonate Level | Typical Use | Effect on the Fabric |
|---|---|---|
| 30–35 PHR | The usual default level with no crease whitening; adjusted slightly for service temperature and color | Balanced processing, flexibility and cost |
| Up to 120 PHR | The usual maximum level | Lower cost, with reduced flexibility and tear strength |
| Up to 160 PHR | Used by some manufacturers to reach the lowest possible cost | Visible crease whitening, brittle hand and shorter service life become likely |
Because filler adds weight without adding strength, a heavily filled fabric can meet a GSM target while falling short on durability. This is one reason GSM alone is not a quality benchmark for PVC coated fabric.
2.5.2 Crease Whitening
Crease whitening, or stress whitening, is the white mark that appears along a fold in PVC coated fabric. Filler level has the strongest influence on it, but other factors play a part:
| Factor | Influence | When Whitening Is More Visible |
|---|---|---|
| Filler | High | Directly proportional: the more filler, the more visible the white marks |
| Plasticizer | Low | Inversely proportional: more visible when plasticizer content is low |
| Ambient Temperature | Medium | Inversely proportional: more visible at low temperatures |
| Weight and Thickness | Low | Less visible when the knife-coated layer is very thin |
| Color | Low | At the same filler level, more visible on green and blue; less visible on beige, light gray and yellow |
Crease whitening matters most for products that are folded, rolled and handled repeatedly, such as truck covers, tents and side curtains. Folding behavior is also checked in our flex resistance testing.
2.5.3 What Filler Tells You About Quality and Cost
If a sample shows clear white marks after folding, feels brittle and tears easily, the filler ratio is usually the most direct cause. This is a key clue when judging the quality of a sample and estimating its cost. When a sample shows no crease whitening, its quality and cost also depend on the resin grade, plasticizer system and processing condition, so one observation alone is not enough to reach a conclusion.
Filler level is also one of the biggest levers on price, so an unusually low quote for the same specification deserves a closer look, especially when comparing vinyl tarp quotes from several suppliers. For durable PVC coated fabric, we set the filler level by the end use, service temperature and color rather than pushing it to the lowest cost.
If you are comparing a sample from another supplier, send it to us. We will evaluate its crease whitening, hand feel and tear behavior, then propose a matched or improved formula and confirm it on a trial sample before bulk production.